Product Details
RTP 0Black
Nylon 6/6 (PA)
Glass Fiber
Heat Stabilized
PROPERTIES & AVERAGE VALUES OF INJECTION MOLDED SPECIMENS
PERMANENCESTANDARD
Primary Additive15%
Density1.26g/cm3ISO 1183
MECHANICAL
Tensile Strength130MPaISO 527
Tensile Elongation3.0 – 4.0%ISO 527
Tensile Modulus6500MPaISO 527
Flexural Strength200MPaISO 178
Flexural Modulus5500MPaISO 178
THERMAL
Heat Deflection Temperature
@ 1.80 MPa240°CISO 75
PROPERTY NOTES
Data herein is typical and not to be construed as specifications.
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.
GENERAL PROCESSING FOR INJECTION MOLDING
Injection Pressure70 – 125MPa
Injection Pressure680 – 1240bar
Melt Temperature275 – 300°C
Mold Temperature65 – 105°C
Drying4 hrs @ 80°C
Moisture Content0.20%
Dew Point-25°C
PROCESSING NOTES
Desiccant Type Dryer Required.
RTP NYLON PA66OTHER TYPES:
RTP 201.3 RC HS13% Glass Fiber Reinforced – Heat Stabilized
RTP 202 RC HS15% Glass Fiber Reinforced – Heat Stabilized
RTP 203 RC HS20% Glass Fiber Reinforced – Heat Stabilized
RTP 204 RC HS25% Glass Fiber Reinforced – Heat Stabilized
RTP 205 RC HS30% Glass Fiber Reinforced – Heat Stabilized
RTP 205.3 RC HS33% Glass Fiber Reinforced – Heat Stabilized
RTP 206 RC HS35% Glass Fiber Reinforced – Heat Stabilized
RTP 207 RC HS40% Glass Fiber Reinforced – Heat Stabilized
RTP 207.3 RC HS43% Glass Fiber Reinforced – Heat Stabilized
RTP 209 RC HS50% Glass Fiber Reinforced – Heat Stabilized
We can give discount according to order quantity.